Beilstein J. Nanotechnol. 2017, 8, 2396–2409, doi:10.3762/bjnano.8.239
Figure 1: Characterization of the NPs used and their calculated deposition on the cellular monolayer. Transmi...
Figure 2: Environmental scanning electron microscopy of J774A.1 macrophages 5 min after NP exposure. Both spe...
Figure 3: Live cell imaging via laser scanning microscopy over 50 min after the onset of NP exposure. AuNPs a...
Figure 4: The intracellular localisation of the NPs 24 h after exposure. (a) Overview showing a part of a cel...
Figure 5: Quantification of uptake by ICP-OES and LSM combined with digital analysis. ICP-OES measurements re...
Figure 6: Mean fluorescence intensity of the intracellular pixels over time. The intensity of the pixels asso...
Figure 7: Time-dependent colocalisation of AuNPs and FeOxNPs with lysosomal markers. The Pearson’s colocalisa...
Figure 8: Colocalisation of AuNPs and FeOxNPs with the lysosomal marker. The interplay of AuNPs, FeOxNPs and ...
Figure 9: Effect of MDC treatment on the uptake of AuNPs and FeOxNPs. The uptake is partially blocked in the ...